Abstract
This article defines quality, quality assurance, quality control, and quality management of processes, products, and services. It describes the evolution of quality control and quality assurance in the coatings industry. The article also discusses the standards, quality programs, and certifications in the coatings industry.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Alison Kaelin, Overview of Quality and the Standards, Programs, and Certifications Used in the Coatings Industry, Protective Organic Coatings, Vol 5B, ASM Handbook, Edited By Kenneth B. Tator, ASM International, 2015, p 32–36, https://doi.org/10.31399/asm.hb.v05b.a0006010
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Quality Control and Quality Assurance
Steel Castings Handbook (Sixth Edition)
Shop and Field Quality Control and Quality Assurance
Protective Organic Coatings
Guidelines for Maintenance Coating of Steel Structures in Pulp and Paper Mills
Protective Organic Coatings
Process Control in the Aluminum Extrusion Plant
Aluminum Extrusion Technology
Design and Certification Considerations
Structural Composite Materials
Specifying Steel Castings
Steel Castings Handbook (Sixth Edition)
Introduction to Testing and Certification
Composites
Accreditation of Mechanical Testing Laboratories
Mechanical Testing and Evaluation
Repair Engineering and Design Considerations
Composites
Sampling
Materials Characterization