Book Chapter
Chapter 19: Microstructure Modeling in Superalloy Forging
By
-
Published:2005
Abstract
This chapter discusses the development and use of microstructure models for optimizing superalloy forging operations. It describes how the processes that control grain structure evolution during hot working were used in model formulation and compares predicted microstructures with experimental results.
You do not currently have access to this chapter.
Citation
Gangshu Shen, Microstructure Modeling in Superalloy Forging, Cold and Hot Forging: Fundamentals and Applications, Edited By Taylan Altan, Gracious Ngaile, Gangshu Shen, ASM International, 2005, p 247–255, https://doi.org/10.31399/asm.tb.chffa.t51040247
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Monte Carlo Models for Grain Growth and Recrystallization
Fundamentals of Modeling for Metals Processing
Nonferrous Metals
Elementary Materials Science
Recovery, Recrystallization, and Grain-Growth Structures
Metallography and Microstructures
Heat Treating of Brasses
Heat Treating of Nonferrous Alloys
Recovery, Recrystallization, and Grain Growth
Elements of Metallurgy and Engineering Alloys
Deformation and Recrystallization of Titanium and Its Alloys
Heat Treating of Nonferrous Alloys
Evolution of Microstructure during Hot Working
Metalworking: Bulk Forming
Textured Structures
Metallography and Microstructures
Modeling and Simulation of Texture Evolution during the Thermomechanical Processing of Titanium Alloys
Fundamentals of Modeling for Metals Processing
Principles of Heat Treating of Nonferrous Alloys
Heat Treating of Nonferrous Alloys