Chapter 18: Process Modeling in Cold Forging Using Finite-Element Analysis
-
Published:2005
Abstract
This chapter discusses the use of finite-element methods for modeling cold forging processes. The discussion covers process modeling inputs, such as geometric parameters, material properties, and interface conditions, and includes several application examples.
You do not currently have access to this chapter.
Citation
Prashant Mangukia, Process Modeling in Cold Forging Using Finite-Element Analysis, Cold and Hot Forging: Fundamentals and Applications, Edited By Taylan Altan, Gracious Ngaile, Gangshu Shen, ASM International, 2005, p 237–246, https://doi.org/10.31399/asm.tb.chffa.t51040237
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
Friction and Lubrication
Cold and Hot Forging Fundamentals and Applications
Process Modeling in Impression-Die Forging Using Finite-Element Analysis
Cold and Hot Forging Fundamentals and Applications
Cold and Warm Forging
Cold and Hot Forging Fundamentals and Applications
Failure in Steel Forging
Failure Analysis of Heat Treated Steel Components
Isothermal and Hot-Die Forging
Metalworking: Bulk Forming
Die Failures in Cold and Hot Forging
Cold and Hot Forging Fundamentals and Applications
Glossary of Terms: Modeling for Metals Processing
Fundamentals of Modeling for Metals Processing
Modeling of Residual Stress and Machining Distortion in Aerospace Components
Metals Process Simulation
Models for Fracture during Deformation Processing
Fundamentals of Modeling for Metals Processing
Process Modeling
Thermal Spray Technology