Abstract
Separation of billets by shearing avoids material loss and is considerably faster than sawing or cutting. This chapter discusses the billet shearing process, the characteristics of sheared surfaces, and the effect of various operating parameters on surface quality. It also includes formulas for calculating shearing force, work, and power and describes various ways to increase production rates.
Serdar Isbir, Pinak Barve, Billet Separation and Shearing, Cold and Hot Forging: Fundamentals and Applications, Edited By Taylan Altan, Gracious Ngaile, Gangshu Shen, ASM International, 2005, p 151–157, https://doi.org/10.31399/asm.tb.chffa.t51040151