Skip Nav Destination
September 12–15, 2022
View ASM Events page>
ASM Technical Books
Cold and Hot Forging: Fundamentals and Applications
Edited by
ASM International
ISBN electronic:
978-1-62708-300-3
Publication date:
2005
Abstract
This chapter discusses the factors that influence temperature in forging operations and presents equations that can be used to predict and control it. The discussion covers heat generation and transfer, the effect of metal flow, temperature measurement, testing methods, and the influence of equipment-related parameters such as press speed, contact time, and tooling geometries.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Gangshu Shen, Temperature and Heat Transfer, Cold and Hot Forging: Fundamentals and Applications, Edited By Taylan Altan, Gracious Ngaile, Gangshu Shen, ASM International, 2005, p 59–66, https://doi.org/10.31399/asm.tb.chffa.t51040059
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Principles of Forging Machines
Cold and Hot Forging Fundamentals and Applications
Temperature Measurement
Steel Metallurgy for the Non-Metallurgist
Temperature Conversions
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Elastic Properties
Materials at Low Temperatures
Tempering Curves
Practical Induction Heat Treating (Second Edition)
Forging and Forming
Titanium: A Technical Guide (Second Edition)
Properties of Gases
Steel Heat Treating Technologies
Forging and Forming
Superalloys: A Technical Guide (Second Edition)
Casting, Forming, and Forging
Gear Materials, Properties, and Manufacture
Primary Working
Titanium Physical Metallurgy, Processing, and Applications