Thermal Spray Technology
Testing of Coatings
-
Published:2013
Abstract
This article describes the two commonly used standardized tests for determining the mechanical properties of thermal spray coatings: hardness testing and tensile adhesion testing. It discusses the destructive and non-destructive methods of residual-stress measurement. Electrochemical testing methodologies include two distinctly different methods: direct and alternating current impedance techniques for assessing the corrosion resistance of coating attributes. The article also reviews the testing methods for determining thermomechanical and environmental stability of thermal barrier coatings. It discusses the wear testing methodologies that are standardized by ASTM, including the pin-on-disk, block-on-ring, dry sand/rubber wheel, erosion, metallographic apparatus abrasion, fretting wear, cavitation, reciprocating ball-on-flat, impact, and rolling contact fatigue test. The article concludes with a discussion on the methods of testing abradability and erosion resistance in abradable coatings.
Walter Riggs, Dana Rucker, Ken Couch, Testing of Coatings, Thermal Spray Technology, Vol 5A, ASM Handbook, Edited By Robert C. Tucker, Jr., ASM International, 2013, p 214–237, https://doi.org/10.31399/asm.hb.v05a.a0005730
Download citation file:
New Handbook: Volume 11B
Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.