Abstract
This article describes post-processing techniques for machining, finishing, heat treating, and deburring used to remove additive manufacturing (AM) metallic workpieces from a base plate and subsequent techniques to enhance printed workpieces. The AM processes include powder bed fusion, binder jetting, and direct energy deposition. The discussion provides information on powder removal, powder recycling and conditioning, part removal, and part enhancement. The mechanism, applications, advantages, and limitations of mechanical, radiation, and chemical-finishing processes as well as the properties of the resulting material are also covered.
Wayne Hung, Post-Processing of Additively Manufactured Metal Parts, Additive Manufacturing Processes, Vol 24, ASM Handbook, Edited By David L. Bourell, William Frazier, Howard Kuhn, Mohsen Seifi, ASM International, 2020, p 298–315, https://doi.org/10.31399/asm.hb.v24.a0006570
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.