Additive Manufacturing Processes
Abstract
The additive manufacturing technologies in the casting of precious metals are divided into two groups: indirect metal methods and direct metal methods. Besides providing a process overview of both of these methods, the focus of this article is on the characteristics, process steps, applications, and advantages of direct metal methods, namely laser melting, material extrusion, binder jetting, material jetting, and vat photopolymerization methods.
Joseph Strauss, Additive Manufacturing of Precious Metals, Additive Manufacturing Processes, Vol 24, ASM Handbook, Edited By David L. Bourell, William Frazier, Howard Kuhn, Mohsen Seifi, ASM International, 2020, p 419–427, https://doi.org/10.31399/asm.hb.v24.a0006556