Abstract
This appendix consists of tables listing temperatures recommended for austenitizing carbon and low-alloy steels prior to hardening.
You do not currently have access to this chapter.
Citation
Austenitizing Temperatures for Steels, Failure Analysis of Heat Treated Steel Components, Edited By Lauralice de C.F. Canale, Rafael A. Mesquita, George E. Totten, ASM International, 2008, p 537–538, https://doi.org/10.31399/asm.tb.fahtsc.t51130537
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Stress-Corrosion Cracking of Carbon and Low-Alloy Steels (Yield Strengths Less Than 1241 MPa)
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
AISI to Non-AISI Steel Cross Reference
Failure Analysis of Heat Treated Steel Components
Classification of Carbon and Low-Alloy Steels
Practical Heat Treating Basic Principles
Hardenability Calculation of Carbon and Low-Alloy Steels with Low or Medium Carbon
Steel Heat Treating Fundamentals and Processes
Dissimilar Welds With Stainless Steels
Welding, Brazing, and Soldering
Failures Related to Welding
Analysis and Prevention of Component and Equipment Failures
Corrosion of Carbon Steel and Low-Alloy Steel Weldments
Corrosion of Weldments
Solidification Structures of Steels and Cast Irons
Metallography and Microstructures
Steel Products and Properties
Metallurgy for the Non-Metallurgist (Second Edition)
Stress Rupture Failures
Failure Investigation of Boiler Tubes A Comprehensive Approach