Failure Analysis of Heat Treated Steel Components
Steel Failures due to Tempering and Isothermal Heat Treatment
-
Published:2008
Abstract
This chapter reviews the causes and cases associated with the problems originated by tempering of steels. To provide background on this phenomenon, a brief description of the martensite reactions and the steel heat treatment of tempering is given to review the different stages of microstructural transformation. A section describing the types of embrittlement from tempering, along with mechanical tests for the determination of temper embrittlement (TE), is presented. Various factors involved in the interaction of the TE phenomenon with hydrogen embrittlement and liquid-metal embrittlement are also provided. The cases covered are grinding cracks on steel cam shaft and transgranular and intergranular crack path in commercial steels.
Jan Vatavuk, L.C.F. Canale, Steel Failures due to Tempering and Isothermal Heat Treatment, Failure Analysis of Heat Treated Steel Components, Edited By Lauralice de C.F. Canale, Rafael A. Mesquita, George E. Totten, ASM International, 2008, p 285–309, https://doi.org/10.31399/asm.tb.fahtsc.t51130285
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.