Carbon Steels and Alloy Steels Used in Warm and Hot Working
-
Published:2014
Abstract
This article focuses on the specific features of carbon steels and alloy steels that are pertinent to heating by induction for warm and hot working processes. It provides a detailed account of the effects of various microstructures on austenitization kinetics for AISI 1045 steels. The article explains the factors to be considered for induction heating of various steel alloys. It describes the temperature and compositional issues that should be considered in the forging of steels that are induction heated.
Chester J. Van Tyne, Kester D. Clarke, Carbon Steels and Alloy Steels Used in Warm and Hot Working, Induction Heating and Heat Treatment, Vol 4C, ASM Handbook, Edited By Valery Rudnev, George E. Totten, ASM International, 2014, p 302–305, https://doi.org/10.31399/asm.hb.v04c.a0005885
Download citation file:
New Handbook: Volume 11B
Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.