Tempering of induction-hardened steel is a form of subcritical heat treatment, primarily carried out to increase ductility, toughness, and dimensional stability, to relieve residual stresses, and to obtain specific values of mechanical properties. This article describes tempering with emphasis on different time-temperature exposure requirements for furnace and induction tempering. It discusses two parametric methods for correlating equivalent time-temperature condition: Hollomon-Jaffe tempering correlation and Grange-Baughman tempering correlation. The article describes different methods of induction tempering, namely, single-shot, progressive or continuous, scanning, and static heating methods. The effects of induction heating variables and hardenability on tempering response are examined. The article also provides examples of how tempering affects the mechanical properties of induction-hardened steels.
Valery Rudnev, Gregory A. Fett, S. Lee Semiatin, Tempering of Induction Hardened Steels, Induction Heating and Heat Treatment, Vol 4C, ASM Handbook, Edited By Valery Rudnev, George E. Totten, ASM International, 2014, p 130–159, https://doi.org/10.31399/asm.hb.v04c.a0005873
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!