Induction Hardening of Gears and Gear-Like Components
-
Published:2014
Abstract
Induction hardening is a prominent method in the gear manufacturing industry due to its ability of selectively hardening portions of a gear such as the flanks, roots, and/or tips of teeth with desired hardness, wearing resistance, and contact fatigue strength without affecting the metallurgy of the core. This article provides an overview of gear technology and materials selection. It describes different gear-hardening patterns, namely, tooth-by-tooth hardening, tip-by-tip hardening, gap-by-gap hardening, spin hardening, single-frequency gear hardening, dual-frequency gear hardening, simultaneous dual-frequency gear hardening, and through heating for surface hardening. It provides information on the different inspection methods based on the...
Sign in
ASM members
Member Sign InValery Rudnev, John Storm, Induction Hardening of Gears and Gear-Like Components, Induction Heating and Heat Treatment, Vol 4C, ASM Handbook, Edited By Valery Rudnev, George E. Totten, ASM International, 2014, p 187–210, https://doi.org/10.31399/asm.hb.v04c.a0005867
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!