Induction Heating Control System
-
Published:2014
Abstract
Induction heating system control is straightforward after the design and application of the coil and power supply required for the job. This article provides an overview of the basic components of an induction heating system, including a machine controller (computer or programmable logic controller), interface wiring, an operator interface, and safety controls. It also provides information on programming devices and temperature controllers, such as manual, auto, and auto-manual temperature controllers.
Sign in
ASM members
Member Sign InMichael Rugg, Induction Heating Control System, Induction Heating and Heat Treatment, Vol 4C, ASM Handbook, Edited By Valery Rudnev, George E. Totten, ASM International, 2014, p 742–745, https://doi.org/10.31399/asm.hb.v04c.a0005854
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field