Induction Case Hardening of Axle Shafts
-
Published:2014
Abstract
This article describes the common types of automotive and truck axle shafts. It provides information on steels used for induction-hardened shafts, and on the manufacturing and induction hardening methods of axle shafts. The article discusses the effects of case depth, shaft length, and carbon content on torsional properties of axle shafts, and the effect of changes in shaft diameter and those of splines on torsional shaft performance. It also provides useful information on straightening and tempering of induction-hardened axle shafts, and describes an effective technique to ensure quality of induction-hardened axle shafts.
Sign in
ASM members
Member Sign InGregory A. Fett, Induction Case Hardening of Axle Shafts, Induction Heating and Heat Treatment, Vol 4C, ASM Handbook, Edited By Valery Rudnev, George E. Totten, ASM International, 2014, p 160–172, https://doi.org/10.31399/asm.hb.v04c.a0005864
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!