Hardness testing equipment is important as all results from the induction equipment are graded by the hardness testing equipment. This article includes maintenance tips and points to consider regarding hardness test equipment, power supplies, controls, programmable logic controllers, computer systems, water cooling systems, fixtures and machines, air-operated or pneumatic devices, coils, and quench systems. It also presents simple rules that need to be applied while moving the equipment from one location to another.
Sign in
ASM members
Member Sign InFred R. Specht, Maintenance of Induction Heat Treating Equipment, Induction Heating and Heat Treatment, Vol 4C, ASM Handbook, Edited By Valery Rudnev, George E. Totten, ASM International, 2014, p 709–713, https://doi.org/10.31399/asm.hb.v04c.a0005850
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!