Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Abstract
Titanium alloys are generally resistant to stress-corrosion cracking (SCC), but under certain conditions, the potential for problems exists. This chapter identifies the types of service environments where titanium alloys have exhibited signs of SCC. It begins by describing the nominal composition, designation, and grade of nearly two dozen commercial titanium alloys and the different types of media (including oxidizers, organic compounds, hot salt, and liquid metal) in which SCC has been observed. It discusses the mechanical and metallurgical factors that influence SCC behavior and examines the cracking and fracture mechanisms that appear to be involved. The chapter also includes...
Sign in
ASM members
Member Sign InStress-Corrosion Cracking of Titanium Alloys, Stress-Corrosion Cracking: Materials Performance and Evaluation, 2nd ed., Edited By Russell H. Jones, ASM International, 2017, p 271–302, https://doi.org/10.31399/asm.tb.sccmpe2.t55090271
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field