This article focuses on the aging characteristics of solution and precipitation heat treated aluminum alloy systems and their corresponding types. It includes information on aluminum-copper systems, aluminum-copper-magnesium systems, aluminum-magnesium-silicon systems, aluminum-zinc-magnesium systems, aluminum-zinc-magnesium-copper systems, and aluminum-lithium alloys.
Heat Treatment Practices of Age-Hardenable Aluminum Alloys, Heat Treating of Nonferrous Alloys, Vol 4E, ASM Handbook, Edited By George E. Totten, ASM International, 2016, p 245–273, https://doi.org/10.31399/asm.hb.v04e.a0006288