Annealing of Refractory Metals
By
John L. Johnson
John L. Johnson
Elmet Technologies LLC
Search for other works by this author on:
-
Published:2016
Abstract
This article briefly discusses the annealing practices for refractory metals such as tungsten, molybdenum, niobium, tantalum, and rhenium and their alloys. It also presents the applications and properties of these metals and their alloys.
You do not currently have access to this chapter.
Citation
John L. Johnson, Annealing of Refractory Metals, Heat Treating of Nonferrous Alloys, Vol 4E, ASM Handbook, Edited By George E. Totten, ASM International, 2016, p 664–666, https://doi.org/10.31399/asm.hb.v04e.a0006255
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
Forging of Refractory Metals
Metalworking: Bulk Forming
Properties and Selection of Powder Metallurgy Refractory Metals
Powder Metallurgy
Special Metallurgical Welding Considerations for Refractory Metals
Welding, Brazing, and Soldering
Properties of Refractory Metal Welds
Weld Integrity and Performance
Refractory Metals
Elements of Metallurgy and Engineering Alloys
Refractory Metal Alloys
Alloying Understanding the Basics
Metallography and Microstructures of Refractory Metals and Alloys
Metallography and Microstructures
Secondary Operations and Quality Control for Refractory Metal Powders
Powder Metallurgy
Machining of Refractory Metals
Machining
Brazing of Refractory and Reactive Metals
Welding, Brazing, and Soldering