Heat Treatable Nonferrous Alloys
-
Published:2016
Abstract
This article describes the different types of precipitation and transformation processes and their effects that can occur during heat treatment of various nonferrous alloys. The nonferrous alloys are aluminum alloys, copper alloys, magnesium alloys, nickel alloys, titanium alloys, cobalt alloys, zinc alloys, and heat treatable silver alloys, gold alloys, lead alloys, and tin alloys. It also provides a detailed discussion on the effects due to precipitation and transformation processes in these non-ferrous alloys.
Alexey Sverdlin, Steven Lampman, Heat Treatable Nonferrous Alloys, Heat Treating of Nonferrous Alloys, Vol 4E, ASM Handbook, Edited By George E. Totten, ASM International, 2016, p 44–62, https://doi.org/10.31399/asm.hb.v04e.a0006274