Heat Treatment of Aluminum Alloy Castings
-
Published:2016
Abstract
This article presents a detailed discussion on typical thermal treatment practices for hardening of various aluminum casting alloys. These practices are solution treatment, quenching or cooling, preaging, and artificial aging at an elevated temperature. The aluminum casting alloys considered here are: Al-Cu and Al-Cu-Mg (2xx) alloys, Al-Zn-Mg (7xx) alloys, Al-Si-Mg alloys, Al-Si-Cu, and Al-Si-Cu-Mg alloys.
Sign in
ASM members
Member Sign InGeoffrey K. Sigworth, Heat Treatment of Aluminum Alloy Castings, Heat Treating of Nonferrous Alloys, Vol 4E, ASM Handbook, Edited By George E. Totten, ASM International, 2016, p 274–288, https://doi.org/10.31399/asm.hb.v04e.a0006264