Heat Treating of Uranium and Uranium Alloys[1]
Reaffirmed
-
Published:2016
Abstract
Heat treatment of depleted uranium (DU) alloys with 4.0 wt% or more molybdenum or equivalent is similar to that of dilute alloys. This article discusses the metallurgical characteristics and processing considerations of DU and its alloys, and describes the control of grain size and orientation using beta treatment. It lists the typical mechanical properties of DU as functions of the amount of cold work and hardness data of uranium rod, and describes the annealing of cold-worked DU. The article also describes the heat treatment of dilute alloys of DU, focusing on the three basic furnace designs used for heating...
Sign in
ASM members
Member Sign InRobert Hackenberg, Heat Treating of Uranium and Uranium Alloys, Heat Treating of Nonferrous Alloys, Vol 4E, ASM Handbook, Edited By George E. Totten, ASM International, 2016, p 667–677, https://doi.org/10.31399/asm.hb.v04e.a0006256
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!