Metallurgy of Titanium Alloy Heat Treatment[1]
Revising author
-
Published:2016
Abstract
This article provides a detailed discussion on the heat treatment processes for titanium and titanium alloys. These processes are age hardening, solution treatment, aging, and annealing. The article illustrates the characteristics of equilibrium phase diagrams that are important for understanding the heat treatment of titanium alloys. It explains the types of metastable phases encountered in titanium alloys. The article also provides information on the equilibrium phase relationships and properties of titanium alloys.
Rodney R. Boyer, John Foltz, Metallurgy of Titanium Alloy Heat Treatment, Heat Treating of Nonferrous Alloys, Vol 4E, ASM Handbook, Edited By George E. Totten, ASM International, 2016, p 498–510, https://doi.org/10.31399/asm.hb.v04e.a0006263