Boiler tube failures associated with material defects are often the result of poor quality control, whether in primary production, on-site fabrication, storage and handling, or installation. This chapter examines quality-related failures stemming from compositional and structural defects, forming and welding defects, design defects, improper cleaning methods, and ineffective maintenance. It also includes case studies and illustrations.