206.0, A206.0, and B206.0[1]: Al-Cu High-Strength Premium Casting Alloys
-
Published:2019
Abstract
The 206.0, A206.0, and B206.0 alloys (aluminum alloys 2xxx) are structural castings in the heat-treated temper for automotive and aerospace applications where high tensile and yield strengths with moderate elongations are needed. This datasheet provides information on key alloy metallurgy and fabrication characteristics of these 2xxx series alloys, as well as the effects of processing on their typical physical and mechanical properties.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
206.0, A206.0, and B206.0: Al-Cu High-Strength Premium Casting Alloys, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 516–519, https://doi.org/10.31399/asm.hb.v02b.a0006555
Download citation file:
Related Book Content
Physical and Mechanical Properties of Select Alloys
Stainless Steels for Design Engineers
Selection and Applications of Magnesium and Magnesium Alloys
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Introduction to Aluminum and Aluminum Alloys
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Introduction and Overview of Copper and Copper Alloys
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Tool Steels
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Pipeline Failure Results from Lightning Strike: Act of Mother Nature?
Handbook of Case Histories in Failure Analysis
Modeling and Simulation of the Heat Treatment of Aluminum Alloys
Heat Treating of Nonferrous Alloys
Hardening and Tempering of Steel
Practical Heat Treating Basic Principles
Heat Treatment of Carbon and Low-Alloy Steels
Practical Heat Treating Basic Principles
Heat Treatment of Tool Steels
Practical Heat Treating Basic Principles