Chain link, a part of a mechanism for transferring hot or cold steel blooms into and out of a reheating furnace, broke after approximately four months of service. The link was cast from 2% Cr austenitic manganese steel and was subjected to repeated heating to temperatures of 455 to 595 deg C (850 to 1100 deg F). Examination included visual inspection, macrograph of a nital-etched specimen from an as-received chain link 1.85x, micrographs of a nital-etched specimen from an as-received chain link 100x/600x, normal microstructure of as-cast standard austenitic manganese steel 100x, micrograph of a nital-etched specimen that had been austenitized 20 min at 1095 deg C (2000 deg F) and air cooled 315x, and micrograph of the same specimen after annealing 68 h at 480 deg C (900 deg F) 1000x). Investigation supported the conclusions that the chain link failed in a brittle manner, because the austenitic manganese steel from which it was cast became embrittled after being reheated in the temperature range of 455 to 595 deg C (850 to 1100 deg F) for prolonged periods of time. The alloy was not suitable for this application, because of its metallurgical instability under service conditions.

You do not currently have access to this chapter.
Don't already have an account? Register

2019. "Conveying Equipment", ASM Failure Analysis Case Histories: Material Handling Equipment

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal