The contamination of lubrication with powdered stone resulted in progressive wear of the internal surfaces of a bearing. Because of the motion of rollers, the inner race exhibited an unusual cyclic washboard wear pattern. Because of a lack of bearing conformity, wear progressed into severe coarse-grain spalling.