Superheater Components
By
H.C. Furtado
;
H.C. Furtado
Centro de Pesquisas de Energia Eletrica-CEPEL
Search for other works by this author on:
Iain Le May
Iain Le May
Metallurgical Consulting Services, Ltd.
Search for other works by this author on:
-
Published:2019
Abstract
Some examples of equipment failures involving high temperature operation are presented. They include some steam generator superheater components and a pump shaft that should not have been at high temperature. Metallographic analysis is used to determine the causes of failure in each case.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
H.C. Furtado, Iain Le May, Superheater Components, ASM Failure Analysis Case Histories: Failure Modes and Mechanisms, ASM International, 2019, https://doi.org/10.31399/asm.fach.modes.c9001688
Download citation file:
Close