The purpose of this investigation was to determine the root cause of the differences noted in the fatigue test data of main rotor spindle assembly retaining rods fabricated from three different vendors, as part of a Second Source evaluation process. ARL performed dimensional verification, accessed overall workmanship, and measured the respective surface roughness of the rods in an effort to identify any discrepancies. Next, mechanical testing was performed, followed by optical and electron microscopy, and chemical analysis. Finally, ARL performed laboratory heat treatments at the required aging temperature and follow-up mechanical testing.

You do not currently have access to this chapter.
Don't already have an account? Register

Marc S. Pepi, Scott M. Grendahl, Victor K. Champagne, Effect of Prior Processing on the Performance of PH 13-8 Mo Stainless Steel Helicopter Components, ASM Failure Analysis Case Histories: Air and Spacecraft, ASM International, 2019, https://doi.org/10.31399/asm.fach.aero.c9001583

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal