Abstract

Several waterwall tubes in a power station boiler failed after ten years of service. The boiler is a suspension type equipped with 30 IK boxes where retractable soot blowers are inserted to clean the inside of the boiler using high-pressure steam. The tubes, which operate at 693 deg F (367 deg C) and 2935 psi (20.5 MPa), failed near the IK boxes as a result of thermal fatigue. Thermal fatigue damage was accelerated by repetitive exposure to water droplets from the soot blower and the associated rapid cooling.

You do not currently have access to this chapter.
Don't already have an account? Register

A. El-Batahgy, W. Metwally, 2019. "Failure Analysis of Boiler Water Wall-Tubes at a Power Generation Plant", ASM Failure Analysis Case Histories: Power Generating Equipment