ASM Failure Analysis Case Histories: Offshore, Shipbuilding, and Marine Equipment documents nearly 30 cases of structural and/or functional failure involving marine engines and propulsion systems, turbines, hulls and structural components, safety and weapon systems, and shipbuilding facilities. The cases describe the investigation, identify the primary cause, and include remedial solutions. These case histories have been compiled from a wide variety of ASM International publication types, including ASM Handbook volumes, conference proceedings, technical books, journals, and magazines.
ASM Failure Analysis Case Histories: Offshore, Shipbuilding, and Marine Equipment
DOI: https://doi.org/10.31399/asm.fach.marine.9781627082273
ISBN (electronic): 978-1-62708-227-3
Publisher: ASM International
Published: 2019
Download citation file:
Table of Contents
-
Breathing Support and Safety Systems
-
Failure Analysis of Pressurized Aluminum Cylinders and Its Applications to a Safer DesignByI. Roman;I. RomanGraduate School of Applied Science and Technology, Materials Science Division, The Hebrew University of JerusalemSearch for other works by this author on:D. RittelD. RittelGraduate School of Applied Science and Technology, Materials Science Division, The Hebrew University of JerusalemSearch for other works by this author on:
-
Engines and Propulsion Systems
-
Broken Connecting Rod from a Motor BoatByEgon KauczorEgon KauczorStaatliches Materialprüfungsamt an der FachhochschuleSearch for other works by this author on:
-
Failure of Nickel-Aluminum-Bronze Hydraulic Couplings, with Comments on General Procedures for Failure AnalysisByS.P. Lynch;S.P. LynchDefence Science and Technology OrganizationSearch for other works by this author on:D.P. Edwards;D.P. EdwardsDefence Science and Technology OrganizationSearch for other works by this author on:R.B. Nethercott;R.B. NethercottDefence Science and Technology OrganizationSearch for other works by this author on:J.L. DavidsonJ.L. DavidsonDefence Science and Technology OrganizationSearch for other works by this author on:
-
-
Marine Turbine Equipment
-
Corrosion Failure of a Heat Exchanger in a Marine EngineByD. A. GuentherD. A. GuentherThe Ohio State UniversitySearch for other works by this author on:
-
Failure of Steam-Water Heat ExchangersByB. F. BrownB. F. BrownU. S. Naval Research LaboratorySearch for other works by this author on:
-
Metallurgical Investigation of a Turbine Blade and a Vane Failure from Two Marine EnginesByA. K. Koul;A. K. KoulStructures and Materials Laboratory, National Aeronautical Establishment, National Research CouncilSearch for other works by this author on:R. V. Dainty;R. V. DaintyStructures and Materials Laboratory, National Aeronautical Establishment, National Research CouncilSearch for other works by this author on:C. MarchandC. MarchandStructures and Materials Laboratory, National Aeronautical Establishment, National Research CouncilSearch for other works by this author on:
-
-
Naval Weapon Systems
-
Shipbuilding Equipment
-
Fractured Post of a Loading GearByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:
-
Structural Components
-
Failure Analysis of TAKR 300 Deck SocketsByXian Jie ZhangXian Jie ZhangCarderock Division Naval Surface Warfare Center Naval Sea Systems CommandSearch for other works by this author on:
-
Failure of Ship Hull Plate Attributed to Lamellar TearingByR. A. MyllymakiR. A. MyllymakiDefense Research Establishment PacificSearch for other works by this author on:
-
Investigation of a Failed Stainless Steel Spindle AssemblyByJ. Morrison;J. MorrisonEsquimalt Defence Research DetachmentSearch for other works by this author on:P.D. MartinP.D. MartinEsquimalt Defence Research DetachmentSearch for other works by this author on:
-
Metallographic Studies of the U.S.S. ArizonaByD.A. MartinezD.A. MartinezU.S.S. Arizona MemorialSearch for other works by this author on:
-
RMS Titanic: A Metallurgical ProblemByH.P. Leighly, Jr.;H.P. Leighly, Jr.University of Missouri-RollaSearch for other works by this author on:S.J. LawrenceS.J. LawrenceBethlehem Steel CorporationSearch for other works by this author on:
-