A 100,000 barrel crude oil storage tank rupture caused extensive property damage in Dec 1980, in Moose Jaw, Saskatchewan. Failure was attributed to a brittle fracture that originated at a weld between a reinforcing pad and a manway nozzle. Factors that contributed to the brittle fracture included incomplete penetration in a single-bevel groove weld, poor impact properties of the hot rolled ASTM A283 low-carbon steel base material, and air temperature down to 27 C on the day of failure. Details of the analysis and results of impact testing are discussed.