Abstract

A four-million gallon capacity (15,142 cu m) oil storage tank ruptured upon filling after re-erection near West Elizabeth, PA on 2 Jan 1988. The tank shell split vertically with failure originating at a flaw existing prior to the reconstruction. Brittle fracture occurred both up and down from the defect when the stress induced by filling reached a critical value for the steel, which had poor toughness properties. This steel had been used in the original construction of a tank in Ohio more than 40 years previously. The defect at which brittle fracture originated in the tank shell showed evidence of burning from a torch. This tank failure was the catalyst for the introduction of new rules concerning the inspection and assessment of older storage tanks.

You do not currently have access to this chapter.
Don't already have an account? Register

I. Le May, C. Bagnall, Failure of a Large Oil Storage Tank, ASM Failure Analysis Case Histories: Oil and Gas Production Equipment, ASM International, 2019, https://doi.org/10.31399/asm.fach.petrol.c9001693

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal