A spoon that was twisted and broken by a person claiming to possess parapsychic powers was submitted for failure analysis. Exemplar tests were conducted on material taken from the bowl region of the same spoon. In addition, tests on other unbroken samples of spoons were evaluated in order to establish both macroscopic and microscopic comparative behavior. These controlled tests produced known failure mechanisms and their respective fracture morphology in this material. A direct comparison could then be made with the unknown failure. The paper identifies a method of analysis that should be applied when analyzing failures of unknown origin.

You do not currently have access to this chapter.
Don't already have an account? Register

W.J.D. Shaw, 2019. "Failure Analysis of a Spoon Broken by a Parapsychic Person", ASM Failure Analysis Case Histories: Household Products and Consumer Goods

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal