A set of plastic grips from an electric consumer product failed while in service. The grips had been injection molded from a general-purpose grade of ABS resin. The parts had cracked while in use after apparent embrittlement of the material. Investigation (visual inspection, SEM imaging, and micro-FTIR in the ATR mode) showed that the spectrum representing the grip surface contained absorption bands associated with ABS as well as additional bands of significant intensity. A spectral subtraction removed the bands associated with the ABS resin resulting in a very good match with glyceride derivatives of fats and oils. This supported the conclusion that the grips failed via brittle fracture associated with severe chemical attack of the ABS resin. A significant level of glyceride derivatives of fatty acids, known to degrade ABS resins, was found on the part surface.

You do not currently have access to this chapter.
Don't already have an account? Register
Close Modal

or Create an Account

Close Modal
Close Modal