Abstract

A 6 x 19 fiber core steel wire rope failed as it was being used to lower a steel television tower. Fracture of the rope occurred at a point under one of two clips used to fashion a spliced loop that was directly connected to the top of the tower. Microscopic examination of the fracture surfaces and the condition of the individual wires revealed that 59% of the wires failed by shear, 39% failed in tension, and 2% had been cut. In addition, 87% of the wires showed some degree of crushing damage, ranging from mild to severe. The failure was attributed to improper installation of the clips.

You do not currently have access to this chapter.
Don't already have an account? Register

Carmine D'Antonio, 1993. "Failure of a Steel Wire Rope From a Television Tower", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul