P. Muraleedharan, J.B. Gnanamoorthy, 1993. "Stress-Corrosion Cracking in a Stainless Steel Emergency Injection Pipe in a Nuclear Reactor", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul