Failure of a Laminated-Paper Food Cooking Tray
By
David O. Leeser
David O. Leeser
Consulting Engineer
Search for other works by this author on:
-
Published:1993
Page range:
480 - 481
Abstract
A laminated-paper microwave food tray collapsed with hot food in it. Microscopic examination of the failed tray revealed no structural or material defects. Five additional trays of like construction were also tested to determine the conditions necessary to simulate the permanent deflection of the tray handles that had occurred in the failed tray. Full distortion of the handles was obtained experimentally only by dropping a full hot tray on its end onto the floor. The test results indicated that the tray had slipped from the hand of the user.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
David O. Leeser, 1993. "Failure of a Laminated-Paper Food Cooking Tray", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul
Download citation file:
Close