Failure of a Sprocket Drive Wheel in a Tracked All-Terrain Vehicle
By
W.A. Pollard
W.A. Pollard
Metals Technology Laboratories, CANMET
Search for other works by this author on:
-
Published:1993
Page range:
58 - 60
Abstract
A sand-cast LM6M aluminum alloy sprocket drive wheel in an all-terrain vehicle failed. Extensive cracking had occurred around each of the six bolt holes in the wheel. Evidence of considerable deformation in this area was also noted. Examination indicated that the part failed because of gross overload. Use of an alloy with a much higher yield strength and improvement in design were recommended.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
W.A. Pollard, 1993. "Failure of a Sprocket Drive Wheel in a Tracked All-Terrain Vehicle", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul
Download citation file:
Close