Durgam G. Chakrapani, 1992. "Intergranular Stress-Corrosion Cracking of Carbon Steel Pipe Welds in a Kamyr Continuous Digester Equalizer Line", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul