There are a wide variety of furnace types and designs for melting aluminum. This article discusses the various types of furnaces, including gas reverberatory furnaces, crucible furnaces, and induction melting furnaces. It describes the classification of solid fluxes: cover fluxes, drossing fluxes, cleaning fluxes, and furnace wall cleaner fluxes. The article reviews the basic considerations in proper flux selection and fluxing practices. It explains the basic principles of degassing and discusses the degassing of wrought aluminum alloys. The article describes filtration in wrought aluminum production and in shape casting. It also reviews grain refinement in aluminum-silicon casting alloys, aluminum-silicon-copper...