This article discusses the failure mechanism of springs. It describes the critical application factors that affect spring fatigue performance. These include: material type and strength; stress conditions; surface quality; manufacturing processes; rate of application of load; and embrittlement or cracking. The article summarizes the methods of statistical analysis of S-N data for general comparisons of fatigue strength of spring steels. The fatigue performance of springs is illustrated by Goodman diagrams. The article also exemplifies the examination of failed springs.