Abstract

This article provides an overview of the electrochemical nature of corrosion and analyzes corrosion-related failures. It describes corrosion failure analysis and discusses corrective and preventive approaches to mitigate corrosion-related failures of metals. These include: change in the environment; change in the alloy or heat treatment; change in design; use of galvanic protection; use of inhibitors; use of nonmetallic coatings and liners; application of metallic coatings; use of surface treatments, thermal spray, or other surface modifications; corrosion monitoring; and preventive maintenance.

You do not currently have access to this chapter.
Don't already have an account? Register

S.R. Freeman, 2002. "Analysis and Prevention of Corrosion-Related Failures", Failure Analysis and Prevention, William T. Becker, Roch J. Shipley