Skip to Main Content

Abstract

This article describes some of the common elemental composition analysis methods and explains the concept of referee and economy test methods in failure analysis. It discusses different types of microchemical analyses, including backscattered electron imaging, energy-dispersive spectrometry, and wavelength-dispersive spectrometry. The article concludes with information on specimen handling.

You do not currently have access to this chapter.
Don't already have an account? Register

Debbie Aliya, 2002. "Chemical Analysis of Metals in Failure Analysis", Failure Analysis and Prevention, William T. Becker, Roch J. Shipley