Abstract

This article discusses the effect of using unsuitable alloys, metallurgical discontinuities, fabrication practices, and stress raisers on the failure of a pressure vessel. It provides information on pressure vessels made of composite materials and their welding practices. The article explains the failure of pressure vessels with emphasis on stress-corrosion cracking, hydrogen embrittlement, brittle and ductile fractures, creep and stress rupture, and fatigue with examples.

You do not currently have access to this chapter.
Don't already have an account? Register

Roy T. King, 2002. "Failures of Pressure Vessels", Failure Analysis and Prevention, William T. Becker, Roch J. Shipley