This article reviews the applied aspects of creep and stress-rupture failures. It discusses the microstructural changes and bulk mechanical behavior of classical and nonclassical creep behavior. The article provides a description of microstructural changes and damage from creep deformation, including stress-rupture fractures. It also describes metallurgical instabilities, such as aging and carbide reactions, and evaluates the complex effects of creep-fatigue interaction. The article concludes with a discussion on thermal fatigue and creep fatigue failures.

You do not currently have access to this chapter.
Don't already have an account? Register

2002. "Creep and Stress Rupture Failures", Failure Analysis and Prevention, William T. Becker, Roch J. Shipley