This article describes the six fundamental factors that decide a tool's performance. These are mechanical design, grade of tool steel, machining procedure, heat treatment, grinding, and handling. A deficiency in any one of the factors can lead to a tool and die failure. The article presents a seven-step procedure to be followed when looking for the reason for a failure. A review of the results of the seven-point investigation may lead directly to the source of failure or narrow the field of investigation to permit the use of special tests.

You do not currently have access to this chapter.
Don't already have an account? Register

2002. "Supplemental Articles", Failure Analysis and Prevention, William T. Becker, Roch J. Shipley