Dual-phase steels are a new class of high-strength low alloy (HSLA) steels characterized by a microstructure consisting of about 20% hard martensite particles dispersed in a soft ductile ferrite matrix. In addition to high tensile strength, in the range of 550 MPa (80 ksi), dual-phase steels exhibit continuous yielding behavior, a low 0.2% offset yield strength, and a higher total elongation than other HSLA steels of similar strength. The article discusses some of the more pertinent aspects of dual-phase steels, such as heat treatment, microstructure, mechanical properties, chemical composition, and manufacturability. In general, these steels have a carbon content...