This chapter covers the failure modes and mechanisms associated with boiler components and the tools and techniques used to assess damages and predict remaining component life. It begins with a review of the design and operation of a utility boiler and the materials used in construction. It then describes the various causes of failure in boiler tubes, headers, and steam pipes, explaining how and why they occur, how they are diagnosed, and how to mitigate their effects. The final and by far largest section in the chapter is a tutorial on damage and life assessment techniques for boiler components...