Book Chapter
Appendix 2: Physical and Mechanical Properties of Select Alloys
-
Published:2008
Abstract
This appendix contains tables listing the physical and mechanical properties of stainless steel engineering alloys. The physical properties covered are density, modulus of elasticity, coefficient of thermal expansion, thermal conductivity, specific heat, and electrical resistivity. The mechanical properties listed include yield strength, tensile strength, elongation and hardness.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Physical and Mechanical Properties of Select Alloys, Stainless Steels for Design Engineers, By Michael F. McGuire, ASM International, 2008, p 279–280, https://doi.org/10.31399/asm.tb.ssde.t52310279
Download citation file:
Related Book Content
Workpiece Materials Database
Metalworking: Bulk Forming
Thermomechanical Testing
Metalworking: Bulk Forming
Thermophysical Properties
Casting
Testing of Stability and Thermal Properties of Thermal Barrier Coatings
Surface Engineering
Modeling and Simulation of Steel Heat Treatment—Prediction of Microstructure, Distortion, Residual Stresses, and Cracking
Steel Heat Treating Technologies
Density of Metals and Alloys
Fundamentals of Modeling for Metals Processing
Growth and Growth-Related Properties of Films Formed by Physical Vapor Deposition
Surface Engineering
Density of Metals and Alloys
Corrosion: Materials
Pipeline Failure Results from Lightning Strike: Act of Mother Nature?
Handbook of Case Histories in Failure Analysis
Modeling and Simulation of the Heat Treatment of Aluminum Alloys
Heat Treating of Nonferrous Alloys